VAE Emulsion(VAE) GW-706
Piav qhia
Saib xyuas
GW-706 VAE hloov yog rauv ntau tshaj ntawm qhov noj thiab yog ib tug txheej lwm muaj ua kev kawg. Rau colleagues, peb tsis muaj npawb xwb ntawm lub xyoo tshaj, yog rauv ntau tshaj ntawm xyoo tshaj, resins, plasticizers, solvents thiab mus nyob rau additiv. Npawb xwb thiab hluas ntawm plasticizer los yog solvent yog hais tsev los yog GW-705 thiab GW-705H hloov, thiab cov npawb xwb solvent, thickener thiab filler yog muaj tau rau thiab yuav tsum muaj npawb xwb thiab hais tsev. Yog li cas li, antifoaming agent QH-81 yog muaj tau rau.
Cov ntaub ntawv thev naus laus zis
Name |
GW-706 |
Cov Ntsiab Lus %≤ |
54.5 |
PH Nqi |
4.0-6.5 |
Viscosity(25℃) Mpa.s |
2500-3500 |
Tos Vam %≤ |
1 |
Dilution Stability %≤ |
3.5 |
Qhov Loj Qho um≤ |
0.2-2.0 |
Qhov Tsawg Tshuaj Tso Tawm Kub ℃≤ |
1 |
Ethylene Ntsiab Lus % |
14-18 |
Pob
50 kg/barrel.
Khaws
VAE Emulsion yuav tsum khaws cia hauv tsev, khaws kom muaj kev nplij siab, qhov kub khaws cia 5-37℃ (yog tias qis dua 0℃, cov khoom yuav txias mus rau hauv lumps lossis txawm tias solidify, thiab tsis yooj yim thaw, txawm tias thawed, nws yooj yim yuav tsim lumps; yog tias qhov kub siab dua 24℃, nws yooj yim yuav ua rau cov khoom saum npoo thickening lossis txawm crust, tab sis nws tseem tuaj yeem siv tom qab tshem tawm cov crust. Yog tias cov khoom tsis tau siv tag nrho tom qab qhib lub hau, nws yuav tsum tau kaw kom zoo tam sim ntawd kom tsis txhob muaj daim tawv.) Lub sijhawm khaws cia ntawm cov khoom yog tsawg dua 180 hnub (nrog rau kev suav los ntawm hnub tsim). Yog tias lub sijhawm khaws cia dhau, nws yuav tsum tau rov tshuaj xyuas raws li tus qauv ua ntej siv.